After printing out the aligners, the supports are removed, and the aligners are cured.(curing time, upward 5 minutes, downward 5 minutes). For other prints, you can cure them after 2 minutes of ultrasonic cleaning with ethanol or IPA.
Each has its pros and cons. In terms of output quality, if you want fast output, then go for a DLP. If you rather want a good quality then, an SLA is suitable.
Check if the output Vat has uneven surfaces. If that’s the case, then you need to even out the vat and If there’s still a problem after that, maybe the parameter is insufficient, or curing has been excessive. You need to adjust the parameters again and try printing.
It is recommended to place it in a well-ventilated, out-of-sunlight location.
And it is recommended to place it stably so that the desk or table does not shake when placed.